For particle size 0 ~30mm, grade between5% to 20% of low grade magnetite and dry powder ore.pre-separation. Improve the grinding quality and reduce the mineral processing cost.
For particle size 0 ~30mm, grade between5% to 20% of low grade magnetite and dry powder ore.pre-separation. Improve the grinding quality and reduce the mineral processing cost.
1the multi-pole is arranged in the internal magnetic system and can increase the stirring of the magnetic particles.
2180°broad-angle magnetic system can effectively improve the iron ore of recovery rate.
3Drum surface used in wear-resistant ceramics, the hardness of HRA is ≥85,can reach HRA92 above.
4Simple material distribution structure, and more convenient to control the fine,tailing grade.